Przeskocz do nawigacji głównej Przeskocz do wyszukiwania Przeskocz do głównej treści

Weldability of the MSRB magnesium alloy

Wyniki badań: Wkład do czasopismaArtykułrecenzja

6 Cytowania z bazy Scopus

Abstrakt

This work, in combination with industrial tests of casting welding, shows that the causes of high-temperature brittleness are the partial tears of the structure and the hot cracks of both the castings, as well as the welded and padded joints. Such phenomena should be treated as irreversible failures caused by the process of crystallization that is in the area of co-existence of the solid and liquid structural constituent. Nil-strength temperature (NST), nil-ductility temperature (NDT) and ductility recovery temperature (DRT) were determined using Gleeble 3800. Obtained results enabled the defining of brittle temperature range of MSR-B magnesium alloy. The assessment of the resistance to hot fractures was conducted on the basis of the transvarestriant trial. The transvarestriant trial involves changing of strain during welding. It was stated that the range of the high-temperature brittleness is very broad, which significantly limits the application of the welding techniques to join or repair elements made of the MSRB alloy. Brittleness is caused mainly by metallurgical factors, i.e. precipitation of intermetallic phases from the solid solution.

Język oryginałuangielski
Strony (od–do)107-118
Liczba stron12
CzasopismoSolid State Phenomena
Tom176
Identyfikatory DOI
Status publikacjiOpublikowano - 30 cze 2011

Obszary tematyczne ASJC Scopus

  • Fizyka atomowa i molekularna oraz optyka
  • Materiałoznawstwo ogólne
  • Fizyka materii skondensowanej

Fingerprint

Zanurz się w tematy badawcze publikacji „Weldability of the MSRB magnesium alloy”. Razem tworzą niepowtarzalny odcisk palca.

Cytowanie