Przeskocz do nawigacji głównej Przeskocz do wyszukiwania Przeskocz do głównej treści

Primary structure and physical properties of new superalloys Co-20Ni-10Al-5Mo-2Nb on Cobalt Matrix

  • Silesian University of Technology
  • Upper Silesian Institute of Technology

Wyniki badań: Wkład do czasopismaArtykułrecenzja

2 Cytowania z bazy Scopus

Abstrakt

In the study we investigated the primary structure and physical properties of the new generation of superalloys based on Co10Al5Mo2Nb type cobalt. The microstructural investigations were carried out with a scanning electron microscope on conventionally prepared electrolytically etched metallographic microsections. The studies of microstructure using a transmission electron microscope were performed using thin films. The testing of mechanical properties in the as-received condition included the performance of static tensile test at room temperature using a testing machine with a maximum load of 200 kN. These materials may replace nickel-based superalloys in the future due to their excellent properties at elevated temperatures relative to nickel-based superalloys. Currently, nickel-strengthened γ′ phase steels are still unrivalled in aerospace applications. However, cobalt-based superalloys are a response to their existing limitations, which do not allow maintaining the current rate of development of aircraft engines.

Język oryginałuangielski
Strony (od–do)129-132
Liczba stron4
CzasopismoActa Physica Polonica A
Tom138
Numer wydania2
Identyfikatory DOI
Status publikacjiOpublikowano - sie 2020

Obszary tematyczne ASJC Scopus

  • Ogólna fizyka i astronomia

Fingerprint

Zanurz się w tematy badawcze publikacji „Primary structure and physical properties of new superalloys Co-20Ni-10Al-5Mo-2Nb on Cobalt Matrix”. Razem tworzą niepowtarzalny odcisk palca.