Abstrakt
Zirconia-sulfate aerogels obtained from the process with the molar hydrolysis ratio r = 4 are more porous and active than those synthesized with r = 2. Sulfate ions markedly hinder sintering of zirconia and structure consolidation during heat treatment and this process depends on their concentration. At a higher sulfate load (20 mol% of SO2-4 in ZrO2) zirconia is amorphous upon calcination at 773 K, irrespective of the water content in the synthesis, while at a lower load it can be crystalline. XRD analysis indicates that the crystalline phase of calcined zirconia-sulfate is cubic and not tetragonal, as observed in conventional zirconia, and reported in previous studies. Acid strength of ZrO2-SO2-4 system appears comparable to that of AlCl3/Al2O3, but lower than that of SbF5/Al2O3.
| Język oryginału | angielski |
|---|---|
| Strony (od–do) | 805-811 |
| Liczba stron | 7 |
| Czasopismo | Polish Journal of Chemistry |
| Tom | 73 |
| Numer wydania | 5 |
| Status publikacji | Opublikowano - 1999 |
Obszary tematyczne ASJC Scopus
- Chemia ogólna
Fingerprint
Zanurz się w tematy badawcze publikacji „Morphology and activity of zirconia-sulfate aerogels”. Razem tworzą niepowtarzalny odcisk palca.Cytowanie
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver