Przeskocz do nawigacji głównej Przeskocz do wyszukiwania Przeskocz do głównej treści

Microstructure and Mechanical Properties of AlSi10MnMg Alloy with Increased Content of Recycled Scrap

  • Freiberg University of Mining and Technology

Wyniki badań: Wkład do czasopismaArtykułrecenzja

7 Cytowania z bazy Scopus

Abstrakt

Increasing the share of circulating scrap in produced castings is not only due to optimizing production costs, but also the need to protect the environment realized by reducing production energy intensity, generating less waste, mitigating greenhouse gas emissions, and consuming fewer natural resources. However, this is associated with maintaining the required properties of castings and considering the impact of impurities on the formation of the structure of aluminum alloys. This research concerns the AlSi10MnMg alloy, which introduces 50 to 75% (every 5%) of circulating scrap. This alloy is one of the most commonly used for producing gravity and pressure die-castings (HPDC), including engine parts and transport structural elements. Based on microscopic research, it was found that the increase in scrap content causes an increase in the share of iron, which results in pre-eutectic (from about 0.45 wt.% to 0.7 wt.% Fe) or even primary crystallization of iron phases (over 0.7 wt.% Fe), mainly the plate–needle phase β-Al5FeSi. Its unfavorable morphology and size cause the formation of numerous shrinkage porosity areas, which has an impact on the reduction in mechanical properties (reduction in UTS and YS by approx. 16% and elongation by approx. 18%, compared to the AlSi10MnMg alloy with 50% scrap content). It was found that the increase in the share of recycled scrap (from 50 to 75%) can be used only when the manganese content is increased. Its effect is to change the morphology of the β-Al5FeSi phase into α-Al15(Fe,Mn)3Si2, whose crystallization occurs in the temperature range of 540 to 555 °C and increases slightly with increasing manganese addition. It is essential to consider the appropriate value of the Mn/Fe quotient, which should be about 1/2, because a higher value may cause the formation of a sludge factor. This work aimed to determine the limiting iron content (contained in the scrap) at which the sequence of the β-Al5FeSi phase release (pre-eutectic or primary crystallization) changes. This sequence mainly affects the form of morphology, the dimensions of the β-Fe phase, and the proportion of shrinkage porosity.

Język oryginałuangielski
Numer artykułu1119
CzasopismoMaterials
Tom18
Numer wydania5
Identyfikatory DOI
Status publikacjiOpublikowano - mar 2025

Cele SDG ONZ

Ten wynik przyczynia się do realizacji następujących celów zrównoważonego rozwoju

  1. Cel 13 - Działanie na rzecz klimatu
    Cel 13 Działanie na rzecz klimatu

Obszary tematyczne ASJC Scopus

  • Materiałoznawstwo ogólne
  • Fizyka materii skondensowanej

Fingerprint

Zanurz się w tematy badawcze publikacji „Microstructure and Mechanical Properties of AlSi10MnMg Alloy with Increased Content of Recycled Scrap”. Razem tworzą niepowtarzalny odcisk palca.

Cytowanie