Mechanically milled al base MMC reinforced with Ti3Al intermetallics

Wyniki badań: Rozdział w książce/raport/materiał konferencyjny › Wkład w konferencję › recenzja

Abstrakt

The present work investigates the structure and selected properties of the aluminum AA 6061 matrix composite materials reinforced with Ti3Al intermetallic particles. The composites were produced by powder metallurgy techniques followed by hot extrusion. The introduction of new reinforcements continues to be investigated in order to improve final behavior of AMCs as well as to avoid some drawbacks of using ceramics as reinforcements. As it is well known that mechanical milling improve characteristics of treated materials, to evaluate the effect of mechanical milling two types of ball mills were used: a low energy (horizontal ball mill) and a high energy one (eccentric ball mill). Basing on the investigations carried out, it was found out that the milling process has a big influence on the characteristics of powder materials, changing their morphology by repeated welding-fracture welding, finally allowing to produce composite particles. The investigation carried out shows that so called brittle intermetallic particles yields to plastic deformation and in the contrary to ceramic particles can not play a role of the accelerator during mechanical milling. The mechanically milled and extruded composites show better mechanical properties of obtained products because of finer and better distribution of reinforcement particles as well as because of the high degree of stress accumulated by plastic deformation. In comparison to composites produced without mechanical milling the hardness increases twice in case of mechanically milled composites. Higher reinforcement content results in higher particles dispersion hardening, for 15 wt. % of intermetallics reinforcement concentration composites reach about 400 MPa UTS. Results of investigation of joints carried out show that the best mechanical properties of joints can be achieved by applying soft conditions of butt welding process e.g. current 1300 A and current flow time 1,2 s. To improve hardness and tensile properties of butt welding joints age hardening is necessary.

Język oryginałuangielski
Tytuł publikacji goszczącejMaterials Science and Technology Conference and Exhibition, MS and T'07 - "Exploring Structure, Processing, and Applications Across Multiple Materials Systems"
WydawcaMaterials Science and Technology
Strony2005-2016
Liczba stron12
ISBN (drukowany)9781605601335
Status publikacjiOpublikowano - 2007
WydarzenieMaterials Science and Technology Conference and Exhibition, MS and T'07 - "Exploring Structure, Processing, and Applications Across Multiple Materials Systems" - Detroit, MI, Stany Zjednoczone
Czas trwania: 16 wrz 2007 → 20 wrz 2007

Seria publikacji

NazwaMaterials Science and Technology Conference and Exhibition, MS and T'07 - "Exploring Structure, Processing, and Applications Across Multiple Materials Systems"
Tom3

Konferencja

KonferencjaMaterials Science and Technology Conference and Exhibition, MS and T'07 - "Exploring Structure, Processing, and Applications Across Multiple Materials Systems"
Kraj/TerytoriumStany Zjednoczone
MiejscowośćDetroit, MI
Okres16/09/07 → 20/09/07

Obszary tematyczne ASJC Scopus

  • Inżynieria przemysłowa i produkcyjna
  • Inżynieria mechaniczna
  • Mechanika materiałowa
  • Materiałoznawstwo ogólne
  • Fizyka materii skondensowanej

Fingerprint

Zanurz się w tematy badawcze publikacji „Mechanically milled al base MMC reinforced with Ti3Al intermetallics”. Razem tworzą niepowtarzalny odcisk palca.

Cytowanie