Isothermal oxidation of additively manufactured and cast 4822 TiAl alloys at 760, 815 and 871 °C

  • Radosław Swadźba
  • , Bogusław Mendala
  • , Lucjan Swadźba
  • , Krzysztof Radwański
  • , Liwia Sozańska-Jędrasik
  • , Łukasz Pyclik
  • , Michele Coppola
  • , Serena Barbieri
  • Lukasiewicz Research Network-Upper Silesian Institute of Technology
  • Avio Polska
  • Avio Aero
  • Avio Aero

Wyniki badań: Wkład do czasopismaArtykułrecenzja

15 Cytowania z bazy Scopus

Abstrakt

The goal of this study was to compare the oxidation behavior of two additively manufactured 48–2–2 TiAl alloys (with banded and not banded microstructures) with a conventionally cast one at 760, 815 and 871 °C. The study focused on the transition from the incubation stage of oxidation to the break-away oxidation that was observed during isothermal oxidation tests. Detailed high resolution STEM investigations were performed to characterize the microstructure, chemistry and phase composition of the oxidation products formed at various stages of oxidation at 760 °C.

Język oryginałuangielski
Numer artykułu111701
CzasopismoCorrosion Science
Tom227
Identyfikatory DOI
Status publikacjiOpublikowano - lut 2024

Cele SDG ONZ

Ten wynik przyczynia się do realizacji następujących celów zrównoważonego rozwoju

  1. Cel 9 - Przemysł, innowacje i infrastruktura
    Cel 9 Przemysł, innowacje i infrastruktura

Obszary tematyczne ASJC Scopus

  • Chemia ogólna
  • Ogólna inżynieria chemiczna
  • Materiałoznawstwo ogólne

Fingerprint

Zanurz się w tematy badawcze publikacji „Isothermal oxidation of additively manufactured and cast 4822 TiAl alloys at 760, 815 and 871 °C”. Razem tworzą niepowtarzalny odcisk palca.

Cytuj to