Przeskocz do nawigacji głównej Przeskocz do wyszukiwania Przeskocz do głównej treści

Improvements of Flexural Properties and Thermal Performance in Thin Geopolymer Based on Fly Ash and Ladle Furnace Slag Using Borax Decahydrates

  • Ng Yong-Sing
  • , Liew Yun-Ming
  • , Heah Cheng-Yong
  • , Mohd Mustafa Al Bakri Abdullah
  • , Phakkhananan Pakawanit
  • , Petrica Vizureanu
  • , Mohd Suhaimi Khalid
  • , Ng Hui-Teng
  • , Hang Yong-Jie
  • , Marcin Nabiałek
  • , Paweł Pietrusiewicz
  • , Sebastian Garus
  • , Wojciech Sochacki
  • , Agata Śliwa
  • Universiti Malaysia Perlis
  • Synchrotron Light Research Institute
  • Gh. Asachi Technical University
  • Technical Sciences Academy of Romania
  • Chemical Services and Environment (Technical Support) Section
  • Częstochowa University of Technology

Wyniki badań: Wkład do czasopismaArtykułrecenzja

15 Cytowania z bazy Scopus

Abstrakt

This paper elucidates the influence of borax decahydrate addition on the flexural and thermal properties of 10 mm thin fly ash/ladle furnace slag (FAS) geopolymers. The borax decahydrate (2, 4, 6, and 8 wt.%) was incorporated to produce FAB geopolymers. Heat treatment was applied with temperature ranges of 300C, 600C, 900C, 1000C and 1100C. Unexposed FAB geopolymers experienced a drop in strength due to a looser matrix with higher porosity. However, borax decahydrate inclusion significantly enhanced the flexural performance of thin geopolymers after heating. FAB2 and FAB8 geopolymers reported higher flexural strength of 26.5 MPa and 47.8 MPa, respectively, at 1000C as compared to FAS geopolymers (24.1 MPa at 1100C). The molten B2O3 provided an adhesive medium to assemble the aluminosilicates, improving the interparticle connectivity which led to a drastic strength increment. Moreover, the borax addition reduced the glass transition temperature, forming more refractory crystalline phases at lower temperatures. This induced a significant strength increment in FAB geopolymers with a factor of 3.6 for FAB8 at 900C, and 4.0 factor for FAB2 at 1000C, respectively. Comparatively, FAS geopolymers only achieved 3.1 factor in strength increment at 1100C. This proved that borax decahydrate could be utilized in the high strength development of thin geopolymers.

Język oryginałuangielski
Numer artykułu4178
CzasopismoMaterials
Tom15
Numer wydania12
Identyfikatory DOI
Status publikacjiOpublikowano - 1 cze 2022

Obszary tematyczne ASJC Scopus

  • Materiałoznawstwo ogólne
  • Fizyka materii skondensowanej

Fingerprint

Zanurz się w tematy badawcze publikacji „Improvements of Flexural Properties and Thermal Performance in Thin Geopolymer Based on Fly Ash and Ladle Furnace Slag Using Borax Decahydrates”. Razem tworzą niepowtarzalny odcisk palca.

Cytowanie