Abstrakt
A comparison of high-temperature corrosion resistance was carried out between Fe40Al5Cr0.2ZrB intermetallic phase-based alloy and TiAl alloy by annealing in air at 1000°C for 50 h, 100 h, 200 h, and 500 h. The extent of oxide scale formation on the surface of both alloys was determined and related to the initial surface condition before the oxidation process. The surfaces of both materials were analyzed and compared after the same annealing time. The surface condition before and after oxidation was examined using a stereoscopic microscope. The kinetics of the oxidation process at 1000°C over a period of 500 h were determined. Samples after oxidation were observed using a Hitachi S-4200 scanning electron microscope. Additionally, energy--dispersive X-ray spectroscopy (EDS) was performed to analyze the chemical composition of all tested samples of both materials after oxidation. The relationship between the occurrence of corrosion products for each of the tested materials and the annealing time was demonstrated.
| Przetłumaczony tytuł wkładu | Wysokotemperaturowe utlenianie stopów na osnowie fazy międzymetalicznej Fe40Al5Cr0,2ZrB i TiAl |
|---|---|
| Język oryginału | angielski |
| Strony (od–do) | 170-174 |
| Liczba stron | 5 |
| Czasopismo | Ochrona Przed Korozja |
| Tom | 66 |
| Numer wydania | 6 |
| Identyfikatory DOI | |
| Status publikacji | Opublikowano - 2023 |
Obszary tematyczne ASJC Scopus
- Ogólna inżynieria chemiczna
- Powierzchnie, powłoki i filmy
- Metale i stopy
- Chemia materiałowa
Fingerprint
Zanurz się w tematy badawcze publikacji „Wysokotemperaturowe utlenianie stopów na osnowie fazy międzymetalicznej Fe40Al5Cr0,2ZrB i TiAl”. Razem tworzą niepowtarzalny odcisk palca.Cytowanie
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver