High martensitic steel after welding with micro-jet cooling in microstructural and mechanical investigations

  • Motor Transport Institute
  • Novar Sp. z o. o.

Wyniki badań: Wkład do czasopismaArtykułrecenzja

7 Cytowania z bazy Scopus

Abstrakt

Modern means of transport will play a significant role in the smart city. In the automotive industry, high-strength steels such as Docol are employed more often. This kind of material is rela-tively not very well weldable. The main reason is related to the Heat Affect Zone, the region in which cracks occur. Another disadvantage is connected with differences in values of ultimate strength of parent and weld material. The differences can be diminished using the correct welding process, which employs nickel and molybdenum electrode wires at much lower sulfur content. The weld metal deposit contains mainly martensite and bainite with coarse ferrite, while the parent material contains mainly martensite and rather fine ferrite. New technology, micro-jet cooling after the joining process enables to obtain the microstructure of weld metal deposit at acceptable parameters. Welding with micro-jet cooling could be treated as a very promising welding Docol steels process with high industrial application. Results of non-destructive inspections on macro samples corre-sponded with further destructive test results (tensile strength, hardness, fatigue, metallographic structure analyses). This article aims to verify fatigue behavior of Docol 1200 M steel after welding supported by the cooling using the micro-jet technique. For the first time, micro-jet cooling was used to weld this kind of steel to check the mechanical properties of the joint, especially to determine the fatigue limit. This study is formulated as follows: investigating fatigue resistance of the Docol 1200 M weld manufactured at the cooling process with micro-jets. The joints were produced in the MAG (Metal Active Gas) technology modified by micro-jet cooling. The results collected in the fatigue test were processed in the form of the Wöhler’s S–N diagram following the fatigue limit of the weld examined. All data have indicated the possibility of obtaining a new method of welded joints with high fatigue limit minimum of 480 MPa. It could be important to achieve a tensile strength of 700 MPa while maintaining the best relative elongation at the level of the base material.

Język oryginałuangielski
Numer artykułu936
Strony (od–do)1-17
Liczba stron17
CzasopismoMaterials
Tom14
Numer wydania4
Identyfikatory DOI
Status publikacjiOpublikowano - 2 lut 2021

Cele SDG ONZ

Ten wynik przyczynia się do realizacji następujących celów zrównoważonego rozwoju

  1. Cel 9 - Przemysł, innowacje i infrastruktura
    Cel 9 Przemysł, innowacje i infrastruktura
  2. Cel 11 - Zrównoważone miasta i społeczności
    Cel 11 Zrównoważone miasta i społeczności

Obszary tematyczne ASJC Scopus

  • Materiałoznawstwo ogólne
  • Fizyka materii skondensowanej

Fingerprint

Zanurz się w tematy badawcze publikacji „High martensitic steel after welding with micro-jet cooling in microstructural and mechanical investigations”. Razem tworzą niepowtarzalny odcisk palca.

Cytowanie