Przeskocz do nawigacji głównej Przeskocz do wyszukiwania Przeskocz do głównej treści

Galvanic corrosion test of magnesium alloys after plastic forming

  • Silesian University of Technology

Wyniki badań: Rozdział w książce/raport/materiał konferencyjnyWkład w konferencjęrecenzja

3 Cytowania z bazy Scopus

Abstrakt

The purpose of this study was to evaluate resistance to galvanic corrosion of magnesium alloys AZ61 and AZ80. Resistance to galvanic corrosion was evaluated with additional application of aluminium alloy 2017A and 8Mn2Si steel as reference materials. The tests were carried out by means of potentiostat VoltaLab PGP 201 by Radiometer with application of Evans method. The tests were carried out in the solution with concentration of 0.01 M NaCl in ambient temperature. For comparison, the relations of the surface of magnesium alloys to aluminium alloys and steel (1:1, 5:1 and 10:1) was differentiated in the experiment. It was proved that AZ80 alloy features slightly higher corrosion resistance in contact with aluminium alloy and steel.

Język oryginałuangielski
Tytuł publikacji goszczącejLight Metals and their Alloys II - Technology, Microstructure and Properties
WydawcaTrans Tech Publications Ltd.
Strony169-176
Liczba stron8
ISBN (drukowany)9783037854655
Identyfikatory DOI
Status publikacjiOpublikowano - 2012

Seria publikacji

NazwaDiffusion and Defect Data Pt.B: Solid State Phenomena
Tom191
ISSN (drukowany)1012-0394

Obszary tematyczne ASJC Scopus

  • Materiały elektroniczne, optyczne i magnetyczne
  • Materiałoznawstwo ogólne
  • Fizyka materii skondensowanej
  • Fizyka i astronomia (różne)

Fingerprint

Zanurz się w tematy badawcze publikacji „Galvanic corrosion test of magnesium alloys after plastic forming”. Razem tworzą niepowtarzalny odcisk palca.

Cytowanie