Abstrakt
Detonation hardening is a high-energy surface modification process; however, the effect of post-hardening heat treatment remains poorly understood. This study addresses this knowledge gap by analysing the synergistic effect of plastic-bonded explosive (PBX) layer thickness (3/4/5/7 mm) and subsequent thermal stress-relief treatment on the microstructure, surface microhardness, and residual-stress state of C45 steel. The experimental results showed a positive but non-proportional relationship between PBX layer thickness and modified-layer depth, which increased from 80 to 100μm, reaching a maximum hardness of 408 HV (a 40% increase over the base material). The most significant finding is that tempering at 150 °C reduced the residual tensile stresses by approximately 52% for the 4 mm PBX variant, while EBSD analysis showed that the refined and morphologically heterogeneous near-surface microstructure remained present after heat treatment. Combined with the residual-stress measurements, these results demonstrate that relatively low-temperature tempering reduced tensile residual stresses while preserving the principal microstructural features produced by detonation hardening.
| Język oryginału | angielski |
|---|---|
| Numer artykułu | 151170 |
| Czasopismo | Materials Science and Engineering: A |
| Tom | 978 |
| Identyfikatory DOI | |
| Status publikacji | Opublikowano - gru 2026 |
Obszary tematyczne ASJC Scopus
- Materiałoznawstwo ogólne
- Fizyka materii skondensowanej
- Mechanika materiałowa
- Inżynieria mechaniczna
Fingerprint
Zanurz się w tematy badawcze publikacji „Effect of PBX layer thickness and tempering postprocessing on the microstructure and mechanical properties of detonation-hardened C45 steel”. Razem tworzą niepowtarzalny odcisk palca.Cytowanie
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver