Abstrakt

Paper presents the assessment of impact of heat treatment on durability in low-cycle fatigue conditions (under constant load) in castings made using post-production scrap of MAR-247 and IN-713C superalloys. Castings were obtained using modification and filtration methods. Additionally, casting made of MAR-247 were subjected to heat treatment consisting of solution treatment and subsequent aging. During low-cycle fatigue test the cyclic creep process were observed. It was demonstrated that the fine-grained samples have significantly higher durability in test conditions and , at the same time, lower values of plastic deformation to rupture Δεpl. It has been also proven that durability of fine-grained MAR-247 samples can be further raised by about 60% using aforementioned heat treatment.

Język oryginałuangielski
Strony (od–do)17-20
Liczba stron4
CzasopismoArchives of Foundry Engineering
Tom15
Numer wydania4
Identyfikatory DOI
Status publikacjiOpublikowano - 1 gru 2015

Obszary tematyczne ASJC Scopus

  • Inżynieria przemysłowa i produkcyjna
  • Metale i stopy

Fingerprint

Zanurz się w tematy badawcze publikacji „Durability of MAR-247 and IN-713C Nickel Superalloys under Cyclic Creep Conditions”. Razem tworzą niepowtarzalny odcisk palca.

Cytowanie