Przeskocz do nawigacji głównej Przeskocz do wyszukiwania Przeskocz do głównej treści

Cyclic oxidation behavior of Ti-Al-C MAX-phase coatings deposited by CHC-PVD on TiAl 48–2–2 at 850 °C

  • R. Swadźba
  • , B. Mendala
  • , L. Swadźba
  • , S. Boubtane ep Zammouri
  • , N. Laska
  • , A. Sasiela
  • , Z. Kania-Pifczyk
  • , K. Ortner
  • , D. Garbiec
  • , J. Wiśniewski
  • Upper Silesian Institute of Technology
  • German Aerospace Center
  • Fraunhofer Institute for Surface Engineering and Thin Films
  • Poznań Institute of Technology

Wyniki badań: Wkład do czasopisma › Artykuł › recenzja

1 Cytowanie z bazy Scopus

Abstrakt

Ti2AlC-based coatings with a thickness of ∼34 μm were synthesized on TiAl 48–2–2 substrates using the closed hollow cathode physical vapor deposition technique at 770 °C, achieving deposition rates of 8–9 μm/h. The coatings consisted predominantly of Ti2AlC with minor Ti3AlC2, as confirmed by room- and high-temperature X-ray diffraction. High resolution transmission electron microscopy and fast Fourier transform analyses showed that the 002 basal planes were oriented predominantly parallel to the growth direction, with local angular deviations associated with V-shaped grain features. Post-deposition high temperature X-ray diffraction demonstrated that the MAX-phase constitution remained unchanged after a 2 h heat treatment at 800 °C in vacuum, confirming the thermal stability of the as-deposited structure. Cyclic oxidation tests at 850 °C (300 × 1 h cycles) revealed degradation behavior consistent with bulk Ti2AlC, initiating at defects such as weld spots and interfacial voids adjacent to V-shaped grains. These voids acted as rapid oxidation pathways, leading to localized Al depletion, TiO2 nucleation, and subsequent breakaway oxidation due to the absence of a continuous, self-healing α-Al2O3 scale. Despite the three-fold increase in thickness compared with our earlier work, the coatings exhibited significantly improved density and microstructural integrity. This study demonstrates that lowering the deposition temperature enables the formation of stable, crystalline MAX-phase coatings with enhanced structural quality, while also clarifying the mechanisms governing their high-temperature oxidation response.

Język oryginałuangielski
Numer artykułu133356
CzasopismoSurface and Coatings Technology
Tom526
Identyfikatory DOI
Status publikacjiOpublikowano - 15 kwi 2026

Obszary tematyczne ASJC Scopus

  • Chemia ogólna
  • Fizyka materii skondensowanej
  • Powierzchnie i interfejsy
  • Powierzchnie, powłoki i filmy
  • Chemia materiałowa

Fingerprint

Zanurz się w tematy badawcze publikacji „Cyclic oxidation behavior of Ti-Al-C MAX-phase coatings deposited by CHC-PVD on TiAl 48–2–2 at 850 °C”. Razem tworzą niepowtarzalny odcisk palca.

Cytowanie