Skip to main navigation Skip to search Skip to main content

The assessment of impact of construction factors on weldability of MSRB alloy

Research output: Chapter in Book/Report/Conference proceedingConference contributionpeer-review

3 Citations (Scopus)

Abstract

The purpose of the work was to assess the impact of construction factors on weldability of MSRB alloy. One conducted transvarestraint test, which allowed to assess welds' susceptibility to cracking under the conditions of forced strain of the casting, Fisco test which simulates welding under the conditions of strong stiffening of the weld, as well as Houldcroft test simulating variable strain of the weld. One concluded that the strain of castings is characteristic of the process of pad welding and welding. Assessment of susceptibility of MSRB alloy to cracking under the conditions of forced strain allows to determine the width of the high-temperature brittleness range (HTBR), critical strain speed of the weld CSS and critical temperature strain intensity CST. These parameters are the criteria of hot cracking of welds from MSRB alloy, therefore, they are indicators of the assessment of the alloy's weldability. Castings from MSRB alloys with constant rigidity should be classified as easily weldable. On the other hand, variable rigidity of the casting, resulting from e.g. diverse thickness of the walls, causes significant increase in the alloy's susceptibility to hot cracking.

Original languageEnglish
Title of host publicationLight Metals Technology V
PublisherTrans Tech Publications Ltd.
Pages37-40
Number of pages4
ISBN (Print)9783037851807
DOIs
Publication statusPublished - 2011

Publication series

NameMaterials Science Forum
Volume690
ISSN (Print)0255-5476
ISSN (Electronic)1662-9752

Keywords

  • Magnesium alloy
  • Repairing of magnesium alloy cast
  • Welding of MSRB

ASJC Scopus subject areas

  • General Materials Science
  • Condensed Matter Physics
  • Mechanics of Materials
  • Mechanical Engineering