Study of casting from IN100 nickel-based superalloy using quantitative metallography and analytical electron miroscopy

Research output: Contribution to journalArticlepeer-review

12 Citations (Scopus)

Abstract

The polycrystalline cast IN100 superalloy was selected for this investigation. It is characterized by dendritic segregation. The major phases which are present in the IN100 superalloy are the ordered γ' (Ni3Al-type) phase together with a disordered solid-solution γ matrix, and carbides. Additionally, a structural element occurs in the microstructure: colonies of (γ + γ') eutectic. The main purpose of this work was to report on the following steps of the IN100 superalloy investigation: specimen preparation with microstructure revealing, image acquisition, computer-aided image analysis with detection of the investigated areas and their measurements. The volume fractions and chemical compositions of the phases were assessed using conventional metallographic and analytical electron microscopy techniques.

Original languageEnglish
Pages (from-to)320-329
Number of pages10
JournalMaterialwissenschaft und Werkstofftechnik
Volume46
Issue number4-5
DOIs
Publication statusPublished - 1 May 2015

Keywords

  • IN100
  • microstructure
  • quantitative metallography
  • superalloy

ASJC Scopus subject areas

  • General Materials Science
  • Condensed Matter Physics
  • Mechanics of Materials
  • Mechanical Engineering

Fingerprint

Dive into the research topics of 'Study of casting from IN100 nickel-based superalloy using quantitative metallography and analytical electron miroscopy'. Together they form a unique fingerprint.

Cite this