Skip to main navigation Skip to search Skip to main content

Structural stability of Mg-6Al-2Sr magnesium alloy

Research output: Contribution to journalArticlepeer-review

5 Citations (Scopus)

Abstract

The Mg-6Al-2Sr magnesium alloy containing 6.15 at.% of aluminium, 2.1 at.% of strontium and 0.42 at.% of manganese was investigated at sand casting state performed at 700°C and after annealing treatment at 180°C, 250°C and 350°C during 500÷5000h with cooling in air. In the as-cast conditions the Mg-6Al-2Sr alloy consisted of α-Mg grains with intermetallic phases: (Al,Mg)4Sr, Al8Mn5 and Al 3Mg13Sr. Annealing at 180°C resulted in the precipitation of the Mg17Al12 phase in the aluminium enriched area and the beginning of decomposition of the Al3Mg 13Sr phase. Annealing at 250°C causes further decomposition of the Al3Mg13Sr phase while no precipitates of the Mg 17Al12 phase could be observed. After exposure at 350°C the total decomposition of the Al3Mg13Sr phase into a mixture of the Al4Sr and α-Mg phases has been observed.

Original languageEnglish
Pages (from-to)75-82
Number of pages8
JournalSolid State Phenomena
Volume176
DOIs
Publication statusPublished - 30 Jun 2011

Keywords

  • Die casting
  • Hardness
  • Mg-6Al-2Sr magnesium alloy
  • Sand casting
  • Structural stability

ASJC Scopus subject areas

  • Atomic and Molecular Physics, and Optics
  • General Materials Science
  • Condensed Matter Physics

Fingerprint

Dive into the research topics of 'Structural stability of Mg-6Al-2Sr magnesium alloy'. Together they form a unique fingerprint.

Cite this