Abstract
In the study we investigated the primary structure and physical properties of the new generation of superalloys based on Co10Al5Mo2Nb type cobalt. The microstructural investigations were carried out with a scanning electron microscope on conventionally prepared electrolytically etched metallographic microsections. The studies of microstructure using a transmission electron microscope were performed using thin films. The testing of mechanical properties in the as-received condition included the performance of static tensile test at room temperature using a testing machine with a maximum load of 200 kN. These materials may replace nickel-based superalloys in the future due to their excellent properties at elevated temperatures relative to nickel-based superalloys. Currently, nickel-strengthened γ′ phase steels are still unrivalled in aerospace applications. However, cobalt-based superalloys are a response to their existing limitations, which do not allow maintaining the current rate of development of aircraft engines.
| Original language | English |
|---|---|
| Pages (from-to) | 129-132 |
| Number of pages | 4 |
| Journal | Acta Physica Polonica A |
| Volume | 138 |
| Issue number | 2 |
| DOIs | |
| Publication status | Published - Aug 2020 |
ASJC Scopus subject areas
- General Physics and Astronomy
Fingerprint
Dive into the research topics of 'Primary structure and physical properties of new superalloys Co-20Ni-10Al-5Mo-2Nb on Cobalt Matrix'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver