N2 - The article describes the process of crystallization of an AlSi17Cu5 (the A3XX.X series according to ASTM standard) alloy which has been modified with 0.05 wt. % P (CuP10 master alloy) and overheated to a temperature of 920°C. It has been shown that, so-called, "time-temperature treatment" (TTT) of alloy in the liquid state, which consists in overheating the alloy to a temperature above Tliq (about 250-300°C), holding at this temperature and rapid cooling, alters the morphology of primary silicon crystals. By the ATD method of thermal analysis, the characteristic temperature of crystallization (Tliq., TEmin., TEmax., TE(Cu), TE(Fe), Tsol.) were determined, and exothermic effects of the modifier and high-degree overheating on the crystallization course of the investigated alloy were examined. A new mechanism of proeutectic crystallization of the α(Al, Me=Cu, Fe) dendrites was proposed. The course of this process is dynamic enough to promote, due to local undercooling, the evolution of heat, which in the ATD curve appears as a well visible additional exothermic effect designated as TX. It is due to the presence in the liquid alloy of microregions with varied content of dissolved silicon.
AB - The article describes the process of crystallization of an AlSi17Cu5 (the A3XX.X series according to ASTM standard) alloy which has been modified with 0.05 wt. % P (CuP10 master alloy) and overheated to a temperature of 920°C. It has been shown that, so-called, "time-temperature treatment" (TTT) of alloy in the liquid state, which consists in overheating the alloy to a temperature above Tliq (about 250-300°C), holding at this temperature and rapid cooling, alters the morphology of primary silicon crystals. By the ATD method of thermal analysis, the characteristic temperature of crystallization (Tliq., TEmin., TEmax., TE(Cu), TE(Fe), Tsol.) were determined, and exothermic effects of the modifier and high-degree overheating on the crystallization course of the investigated alloy were examined. A new mechanism of proeutectic crystallization of the α(Al, Me=Cu, Fe) dendrites was proposed. The course of this process is dynamic enough to promote, due to local undercooling, the evolution of heat, which in the ATD curve appears as a well visible additional exothermic effect designated as TX. It is due to the presence in the liquid alloy of microregions with varied content of dissolved silicon.
KW - Hypereutectic silumins
KW - Modification
KW - Overheating
KW - Proeutectic crystallization
UR - https://www.scopus.com/pages/publications/84891475567
U2 - 10.4028/www.scientific.net/SSP.212.237
DO - 10.4028/www.scientific.net/SSP.212.237
M3 - Conference contribution
AN - SCOPUS:84891475567
SN - 9783037859452
T3 - Solid State Phenomena
SP - 237
EP - 242
BT - Technologies and Properties of Modern Utility Materials XXI
PB - Trans Tech Publications Ltd.
T2 - 21st Conference on Technologies and Properties of Modern Utility Materials, TPMUM 2013
Y2 - 17 May 2013 through 17 May 2013
ER -