Abstract
The Ca,Eu-α-sialon powders with the mixed solid solution composition have been manufactured via the solid-state reaction process in flowing nitrogen in a graphite furnace at a relatively low temperature of 1650 °C without an external overpressure. XRD data with Rielveld refinement and XPS measurements were used for characterization of the lattice constants and the surface chemical composition. The monophase Ca-Eu-α-sialon was obtained with the nominal composition of Eu0.048Ca0.702Si7.75Al2.25O0.75N15.25. The highest emission intensity in a yellow-orange region at 590 nm and quantum efficiency of 66% was found for this pure Ca,Eu-α-sialon. Estimation of m,n values from the lattice constant and EDS results showed a small deviation from the nominal composition of designed α-sialon. XPS results demonstrated significant changes of the chemical composition in the oxidized surface of phosphor particles. Possible reasons of emission redshift and relationship between the actual solid solution composition and luminescence properties are discussed in terms of simultaneous presence of Eu2+ and Eu3+ ions in the sialon crystal lattice and residual oxynitride glass.
| Original language | English |
|---|---|
| Pages (from-to) | 43-48 |
| Number of pages | 6 |
| Journal | Optical Materials |
| Volume | 59 |
| DOIs | |
| Publication status | Published - 1 Sept 2016 |
Keywords
- Ca,Eu-α-sialon
- Eu oxidation state
- Photoluminescence
- Solid solution
ASJC Scopus subject areas
- Electronic, Optical and Magnetic Materials
- General Computer Science
- Atomic and Molecular Physics, and Optics
- Spectroscopy
- Physical and Theoretical Chemistry
- Organic Chemistry
- Inorganic Chemistry
- Electrical and Electronic Engineering
Fingerprint
Dive into the research topics of 'Luminescence properties of the Ca-alpha-sialon:Eu solid solution'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver