Abstract

High temperature corrosion is currently one of the main causes of failures in utility boilers. In particular, in recent years, low NOx corrosion of waterwalls in the area of the burner belt has caused a significant decrease in the lifetime of tubes. Before the introduction of low NOx combustion methods, the lifetime of waterwalls exceeded 10 or more years, while now it does not exceed 5 - 6 years. The fireside waterwall wear is commonly linked with a lack of oxygen and a high CO concentration in the flue gas accompanied with the presence of sulfur and chlorine compounds. Such conditions are inevitable while using primary NOx reduction methods in coal-fired boilers. The amount of chlorine in the coals used in Polish power plant boilers is rather low (commonly Clr 0,2 %) and therefore the predominant corrosion mechanism is the attack of gas phase H2S, a product of reactions in ash deposits containing sulfur compounds. The paper presents a new equation for calculating low-NOx corrosion rate as well as an exemplary calculation presented as the isolines of tube thickness loss [nm/h] over the rear waterwall in the boiler of the ERSA power plant.

Original languageEnglish
Pages (from-to)121-128
Number of pages8
JournalRynek Energii
Volume91
Issue number6
Publication statusPublished - 2010

Keywords

  • Boiler
  • Kinetics
  • Low NOx corrosion
  • Waterwalls

ASJC Scopus subject areas

  • General Mathematics
  • General Energy

Fingerprint

Dive into the research topics of 'Kinetics of low nox corrosion of waterwalls in utility boilers'. Together they form a unique fingerprint.

Cite this