Abstract
This paper presents the results of tests conducted on the HR6W (23Cr-45Ni-6W-Nb-Ti-B) alloy under low-cycle fatigue at room temperature and at 650◦ C. Fatigue tests were carried out at constant values of the total strain ranges. The alloy under low-cycle fatigue showed cyclic strengthening both at room temperature and at 650◦ C. The degree of HR6W strengthening described by coefficient n’ was higher at higher temperatures. At the same time, its fatigue life Nf at room temperature was, depending on the range of total strain adopted in the tests, several times higher than observed at 650◦ C.
| Original language | English |
|---|---|
| Article number | 6741 |
| Journal | Materials |
| Volume | 14 |
| Issue number | 22 |
| DOIs | |
| Publication status | Published - 1 Nov 2021 |
Keywords
- Cyclic strengthening curve
- Fatigue life
- HR6W alloy
- Low-cycle fatigue
ASJC Scopus subject areas
- General Materials Science
- Condensed Matter Physics
Fingerprint
Dive into the research topics of 'Impact of temperature on low-cycle fatigue characteristics of the HR6W alloy'. Together they form a unique fingerprint.Cite this
- APA
- Author
- BIBTEX
- Harvard
- Standard
- RIS
- Vancouver