Fiber laser welding of nickel based superalloy Rene 77

Research output: Chapter in Book/Report/Conference proceeding › Conference contribution › peer-review

25 Citations (Scopus)

Abstract

The study of laser bead-on-plate welding of nickel based superalloy Rene 77 using single mode high power fiber laser has been undertaken to determine the effect of process parameters, such as laser power, welding speed and laser beam defocusing, on the weld geometry and quality. Non-porous and crack-free welds can be achieved for a relatively wide range of fiber laser welding parameters. The welding speed has a major effect on the weld aspect ratio. The laser beam defocusing significantly affects the weld bead geometry, the stability of the keyhole and pore formation. The transition from keyhole mode to conduction mode welding occurs between focal point position +2.0 mm and +4.0 mm. The high porosity was observed at the focal point position of +2.0 mm. The heat input higher than18 J/mm results to hot cracking in the heat affected zone (HAZ). Moreover, it was found that the welds with the weld aspect ratio higher than 1.5 contain cracks, which propagate from the HAZ into the weld metal.

Original languageEnglish
Title of host publicationLaser Technology 2012
Subtitle of host publicationApplications of Lasers
DOIs
Publication statusPublished - 2013
EventLaser Technology 2012: Applications of Lasers - Szczecin - Swinoujscie, Poland
Duration: 24 Sept 2012 → 28 Sept 2012

Publication series

NameProceedings of SPIE - The International Society for Optical Engineering
Volume8703
ISSN (Print)0277-786X

Conference

ConferenceLaser Technology 2012: Applications of Lasers
Country/TerritoryPoland
CitySzczecin - Swinoujscie
Period24/09/12 → 28/09/12

Keywords

  • Rene 77
  • fiber laser
  • laser welding
  • nickel based superalloy

ASJC Scopus subject areas

  • Electronic, Optical and Magnetic Materials
  • Condensed Matter Physics
  • Computer Science Applications
  • Applied Mathematics
  • Electrical and Electronic Engineering

Fingerprint

Dive into the research topics of 'Fiber laser welding of nickel based superalloy Rene 77'. Together they form a unique fingerprint.

Cite this